(!)NOTE : Windows 7 users won’t be able to use some latest features of eCatalog/WOS since Microsoft is ending support for Windows 7 on 14 Jan, 2020. Please upgrade your system for uninterrupted services.

  • Viewed
    Products
  • My
    Components
  • Cart
Recently Viewed Products
X
My Components
X
Cart item(s)
X
Loading...
  • Due to an increase in demand, the lead time of some of the electrical items from our eCatalogue has increased abnormally and may cause delays in delivery or order suspension. We apologize for the inconvenience and appreciate your kind understanding. Once the supply will get normalized, we will update the same.

Welding gauge AWG-10

Welding gauge AWG-10

Click this image to zoom it.

Move the mouse over or click the image to zoom

You can add up to 6 items per a category to the compare list.

Part Number :
    • Starting From :
      3,255₹/Unit
  • Order Qty :
  • Total Price :
    ---
  • Days to ship :
    ---

Select part number to Order Now/ Add to Cart

Product Description

Dedicated analog type gauge for measuring throat depth of fillet and height of excess weld metal. An essential item for welding processes.
[Features]
· Made of stainless steel for simple anti-rust treatment.
· Beveling angle: 60°, 70°, 80°, 90°.
· Fillet throat thickness: 11 mm.
· Height of excess weld metal: 8 mm.
· Instrument difference: ±0.2 mm.
· Minimum read value: 0.1 mm.
[Applications]
· Used to determine the size of weld overlay and fillet.

What is welding gauge

Welding gauge is used to measure and check size of welded part throat
thickness required strength split that may casue damage irregularity of
under-cut and overlap etc.
 

Terms of welding

  • Throat thickness
    The thickness from welded portion at triangular cross-section when welding two faces at 90°.
  • Arc strike
    The arc that occurred to parts other than welding base metal when working on arc welding.
  • Pit
    Blow hole on surface due to poor welding.
  • Bead
    A belt shape rises after working on welding.
  • Under-Cut
    The irregular groove at the toe of a rod in the welding base metal.
  • Overlap
    The heap results from miss welding of the base metal.


Instructions for inspection

Inspection itemsPictureinstruction for measuring
Reasons of welding crack
1.Surface crack
on bead
Visual inspectin in priciple
Inspection of exterior and shape on welding bead
2.Pit on welding bead surfaceVisual inspection
3.Unevenness on welding bead surface
4.Under-cut
5.OverlapVisual inspection
6.Size of corner buds (Lack of throat thickness • foot length of fillet)
7.Excessive buds from groove welding
Others
8.Arc strikeVisual inspection
Part Number
AWG-10
Part NumberPriceMinimum Order Qty.Volume DiscountDays to Ship

₹ 3,255.07

1 Piece(s) 10 Day(s) or more

Loading...

  1. 1
 

Basic Information

Measuring Range(mm) 11 Minimum Read Value(mm) 0.1 Dimensions Measurement Accuracy(mm) ±0.2
Measuring bevel angle / groove angle(°) 60°、70°、80°、90° Mass(g) 80 Material Stainless Steel
Feature 1 · Made with stainless steel for easy anti-rust processing Use Weld Overlay, Fillet Size